• SAE USCAR5-5

SAE USCAR5-5

AVOIDANCE OF HYDROGEN EMBRITTLEMENT OF STEEL FASTENERS AND OTHER HARDENED OR SPRING STEEL PARTS FROM SURFACE COATING PROCESSES

SAE International , 02/27/2019

Publisher: SAE

File Format: PDF

$31.00$63.00


This standard outlines the conditions that enhance the risk of hydrogen embrittlement of steel and defines the relief procedures required to minimize the risk of hydrogen embrittlement. It is intended to control the process.

Hydrogen embrittlement of steel, which can cause brittle fractures under stress, occurs as a result of the absorption of hydrogen during cleaning, phosphate coating and plating processes. The susceptibility to hydrogen embrittlement increases with increasing stress (internal or externally applied stress) and increasing material strength.

Hardness readings in this specification are in Vickers scale. SAE J417 should be referred to for conversion to other scales.

SAE USCAR5-5 History

SAE USCAR5-5

SAE USCAR5-5

$31.00 $63.00

SAE USCAR5-4

SAE USCAR5-4

$25.00 $50.00

SAE USCAR5-3

SAE USCAR5-3

$25.00 $50.00

More SAE Standards PDF

SAE AMS4782G

SAE AMS4782G

$28.00 $56.00

SAE AMS4779H

SAE AMS4779H

$28.00 $56.00

SAE AMS4041R

SAE AMS4041R

$30.00 $61.00

SAE AS81969/30A

SAE AS81969/30A

$37.00 $74.00